| STRUCTURE |
Cr |
| SPECIFIC DENSITY |
1.04 |
| WATER ABSORBTION RATE (%) |
0.4 |
| ELONGATION (%) |
300 |
| TENSILE STRENGTH (psi) |
8000 |
| COMPRESSION STRENGTH (psi) |
7900 |
| FLEXURAL STRENGTH (psi) |
6000 |
| FLEXURAL MODULUS (psi) |
145000 |
| IMPACT (IZOD ft. lbs/in) |
1.8 |
| HARDNESS |
R108 |
| FABRICATION |
- - BONDING: G
- - ULTRASONIC WELDING: P
- - MACHINING: P
|
| DEFLECTION
TEMPERATURE (deg. F) |
- - @ 66 psi: 266
- - @ 264 psi: 302
|
| UTILZATION
TEMPERATURE (deg. F) |
|
|
| MELTING POINT (deg. F) |
365 |
| COEFFICIENT OF EXPANSION |
0.000072 |
| ARC RESISTANCE |
120 |
| DIELECTRIC STRENGTH (kV/mm) |
17 |
| TRANSPARENCY |
O |
| UV RESISTANCE |
G |
| CHEMICAL
RESISTANCE |
- - ACIDS: P
- - ALKALIS: P
- - SOLVENTS: G
|