| STRUCTURE |
Cr |
| SPECIFIC DENSITY |
1.23 |
| WATER ABSORBTION RATE (%) |
0.3 |
| ELONGATION (%) |
5 |
| TENSILE STRENGTH (psi) |
13500 |
| COMPRESSION STRENGTH (psi) |
16000 |
| FLEXURAL STRENGTH (psi) |
4400 |
| FLEXURAL MODULUS (psi) |
360000 |
| IMPACT (IZOD ft. lbs/in) |
4.4 |
| HARDNESS |
R110 |
| FABRICATION |
- - BONDING: G
- - ULTRASONIC WELDING: G
- - MACHINING: P
|
| DEFLECTION
TEMPERATURE (deg. F) |
- - @ 66 psi: 230
- - @ 264 psi: 300
|
| UTILZATION
TEMPERATURE (deg. F) |
|
|
| MELTING POINT (deg. F) |
350 |
| COEFFICIENT OF EXPANSION |
0.000016 |
| ARC RESISTANCE |
120 |
| DIELECTRIC STRENGTH (kV/mm) |
17 |
| TRANSPARENCY |
O |
| UV RESISTANCE |
G |
| CHEMICAL
RESISTANCE |
- - ACIDS: P
- - ALKALIS: P
- - SOLVENTS: G
|