| STRUCTURE |
Cr |
| SPECIFIC DENSITY |
1.14 |
| WATER ABSORBTION RATE (%) |
1.3 |
| ELONGATION (%) |
150 |
| TENSILE STRENGTH (psi) |
7600 |
| COMPRESSION STRENGTH (psi) |
8700 |
| FLEXURAL STRENGTH (psi) |
5800 |
| FLEXURAL MODULUS (psi) |
200000 |
| IMPACT (IZOD ft. lbs/in) |
2.1 |
| HARDNESS |
R100 |
| FABRICATION |
- - BONDING: G
- - ULTRASONIC WELDING: P
- - MACHINING: G
|
| DEFLECTION
TEMPERATURE (deg. F) |
- - @ 66 psi: 390
- - @ 264 psi: 250
|
| UTILZATION
TEMPERATURE (deg. F) |
|
|
| MELTING POINT (deg. F) |
490 |
| COEFFICIENT OF EXPANSION |
0.000044 |
| ARC RESISTANCE |
130 |
| DIELECTRIC STRENGTH (kV/mm) |
18 |
| TRANSPARENCY |
T |
| UV RESISTANCE |
G |
| CHEMICAL
RESISTANCE |
- - ACIDS: P
- - ALKALIS: P
- - SOLVENTS: G
|