| STRUCTURE |
Cr |
| SPECIFIC DENSITY |
1.37 |
| WATER ABSORBTION RATE (%) |
0.15 |
| ELONGATION (%) |
70 |
| TENSILE STRENGTH (psi) |
6600 |
| COMPRESSION STRENGTH (psi) |
14000 |
| FLEXURAL STRENGTH (psi) |
16000 |
| FLEXURAL MODULUS (psi) |
400000 |
| IMPACT (IZOD ft. lbs/in) |
0.8 |
| HARDNESS |
R120 |
| FABRICATION |
- - BONDING: G
- - ULTRASONIC WELDING: G
- - MACHINING: E
|
| DEFLECTION
TEMPERATURE (deg. F) |
- - @ 66 psi: 330
- - @ 264 psi: 212
|
| UTILZATION
TEMPERATURE (deg. F) |
|
|
| MELTING POINT (deg. F) |
480 |
| COEFFICIENT OF EXPANSION |
0.000039 |
| ARC RESISTANCE |
80 |
| DIELECTRIC STRENGTH (kV/mm) |
20 |
| TRANSPARENCY |
|
| UV RESISTANCE |
G |
| CHEMICAL
RESISTANCE |
- - ACIDS: G
- - ALKALIS: G
- - SOLVENTS: G
|